1-200 m³ steel-lined PTFE storage tank_SupplyPro Co., Ltd._Wuxi Huashun Anticorrosion Container Technology Co., Ltd. 
在线客服 在线客服邀请中...
关闭

您好,现在客服正邀请与您通话,请留下您的联系方式,客服将尽快与您取得联系。

 点击提交代表您同意《服务条款》《隐私政策》
13921511789
 

Product Categories
  • No Category

Contact Information
  • Contact person:张总
  • Telephone:13921511789
  • Mobile:13921511789
  • Address:38 Luoyang North Road, Shuangmiao Village, Luoshi Town, Wuxi City, Huishan District
Home > SupplyPro Co., Ltd. > 1-200 m³ steel-lined PTFE storage tank
1-200 m³ steel-lined PTFE storage tank
品牌: Huashun
Origin: Wuxi
Custom Processing & Tailoring: Sure
Performance: Corrosion-resistant, leak-proof, and peel-resistant
单价: 电议
最小起订Quantity:
供货总Quantity:
有效期至: 长期有效
最后更新: 2025-05-09 14:22
 
详细Info

Pre-treatment

The inner surface of the lining equipment is degreased with solvents and dried, followed by sandblasting with 46# steel grit. The surface that has been sandblasted is then cleaned with trichloroethylene and dried.

Surface paint treatment

Section 3: Adhesive Coatings

A layer of special adhesive is evenly coated on the inside surface of the product, and a layer of adhesive is also applied to the back of the composite board. Then, align the positions and affix the composite board.

Four, stickiness

After aligning the adhesive-coated composite panels, affix them in place first. Then, apply local heat and roll to expel air trapped in between, ensuring a closer fit for the 3mm or 4mm polytetrafluoroethylene sheets.

Five: Weld Seam

Once the composite panels are fully bonded, use a professional notching machine to create "V" shaped long grooves at the junction of the two panels, and clean out any impurities in the gaps.

Welding

Utilize imported high-temperature welding torches with Φ3.5mm PFA welding rods. Weld the two composite panels together in the center of the grooved seam, ensuring no impurities, bubbles, or incomplete welds. After the overall welding is complete, use a pinhole tester to test with 15,000 volts to check for any microholes and make necessary repairs. Upon completion of the inspection, flatten any protruding welding rods on the composite panel's top surface using an imported groove planer. Then, reinforce the original welding rods with a 20mm-wide welding strip to ensure a secure and bubble-free weld. Finally, test for pinholes with a 30,000-volt voltage after welding is finished to further confirm the welding quality.

Section 7: Inspection