Stainless Steel Lined PTFE Lined Storage Tanks_SupplyPro Co., Ltd._Wuxi Huashun Anticorrosion Container Technology Co., Ltd. 
在线客服 在线客服邀请中...
关闭

您好,现在客服正邀请与您通话,请留下您的联系方式,客服将尽快与您取得联系。

 点击提交代表您同意《服务条款》《隐私政策》
13921511789
 

Product Categories
  • No Category

Contact Information
  • Contact person:张总
  • Telephone:13921511789
  • Mobile:13921511789
  • Address:38 Luoyang North Road, Shuangmiao Village, Luoshi Town, Wuxi City, Huishan District
Home > SupplyPro Co., Ltd. > Stainless Steel Lined PTFE Lined Storage Tanks
Stainless Steel Lined PTFE Lined Storage Tanks
品牌: Hua Shi Shun
Origin: Wuxi
Custom Processing: Is
Performance: Corrosion-resistant, leak-proof, and peel-resistant
单价: 电议
最小起订Quantity:
供货总Quantity:
有效期至: 长期有效
最后更新: 2025-05-09 14:22
 
详细Info

Steel-lined PTFE Lined Storage Tanks, Vertical and Horizontal Mixers Storage Tanks

Pre-treatment

The inner surface of the lining equipment is first degreased with solvents and dried, followed by sandblasting with 46# steel grit. The surface is then cleaned with trichloroethylene and dried.

Section 2: Bottom Paint Treatment

Section 3: Adhesive Coating

Apply a uniform layer of special adhesive inside the product, and also coat the backside of the composite panel with adhesive. Then, align and affix the composite panel in place.

Four, Paste

After aligning the adhesive-coated composite panel, first apply it in place. Then, perform local heating and rolling to expel air trapped between layers, ensuring a closer fit for the 3mm or 4mm PTFE (Teflon) sheet.

Five. Weld Seam

Once all the composite panels are bonded, use a professional notching machine to create "V" shaped grooves at the junction of the two panels, and clean out any debris from the gaps.

Welding

Utilize imported high-temperature welding torch with Φ3.5mm PFA welding rods. Weld the two composite panels together in the middle of the grooved seam, ensuring there are no impurities, bubbles, or incomplete welds. After the overall welding is complete, use a pinhole tester to test at 15,000 volts for any microholes and make necessary repairs. Upon completion of the inspection, flatten any protruding welding rods on the composite panel's upper surface using an imported groove planer. Then, reinforce the original welding rods with a 20mm-wide welding strip to ensure the welds are secure and free of microholes. Finally, test for pinholes with a 30,000-volt voltage after welding is finished to further confirm the welding quality.

Seven: Inspection