1-200m³ Stainless Steel Lined PTFE Storage Tank_SupplyPro Co., Ltd._Wuxi Huashun Anticorrosion Container Technology Co., Ltd. 
在线客服 在线客服邀请中...
关闭

您好,现在客服正邀请与您通话,请留下您的联系方式,客服将尽快与您取得联系。

 点击提交代表您同意《服务条款》《隐私政策》
13921511789
 

Product Categories
  • No Category

Contact Information
  • Contact person:张总
  • Telephone:13921511789
  • Mobile:13921511789
  • Address:38 Luoyang North Road, Shuangmiao Village, Luoshi Town, Wuxi City, Huishan District
Home > SupplyPro Co., Ltd. > 1-200m³ Stainless Steel Lined PTFE Storage Tank
1-200m³ Stainless Steel Lined PTFE Storage Tank
品牌: Hua Shi Shun
Origin: Wuxi
Custom Processing: Certainly
Performance: Corrosion-resistant, leak-proof, and non-flaking
单价: 电议
最小起订Quantity:
供货总Quantity:
有效期至: 长期有效
最后更新: 2025-05-09 14:22
 
详细Info

Pre-treatment

The inner surface of the lining equipment is degreased with solvents and dried, followed by sandblasting with 46# steel grit. The surface that has been sandblasted is then cleaned with trichloroethylene and dried.

Two, Base Paint Treatment

Section 3: Adhesive Coating

The product is evenly coated with a special adhesive inside, and the back of the composite panel is also coated with adhesive. Then, align the positions and affix the composite panel.

Four,粘贴

After aligning the adhesive-coated composite panels in the correct position, apply them first. Then, use local heating and rolling to expel the air trapped in between, ensuring a tighter fit for the 3mm or 4mm polytetrafluoroethylene sheets.

Five: Weld Seam

After all the composite boards are fully bonded, use a professional notching machine to create a "V" shaped long groove at the junction of the two composite boards, and clean out any debris from the gap.

Welding

Utilize imported high-temperature welding torches with Φ3.5mm PFA welding rods. Weld the two composite panels together in the middle of the grooved seam, ensuring there are no impurities, bubbles, or missed welds. After the overall welding is complete, use a pinhole tester to test with 15,000 volts to check for any microholes and make necessary repairs. Upon completion of the inspection, flatten any protruding welding rods on the composite panel's top surface using an imported groove planer. Then, reinforce the original welding rods with a 20mm-wide welding strip to ensure the welds are secure and free of microholes. Finally, test for pinholes with a 30,000-volt voltage after welding is finished to further confirm the welding quality.

Section 7: Inspection