    Three Common Questions About Teflon Coating

    2025-08-15

    Today, Chongqing Teflon Coating is here to discuss the three common issues with Teflon coating and their solutions.

    Phenomenon: Granulation, Spraying

    Reason: Teflon Coating Experts Explain - Unclean work sites lead to dust mixed with paint; paint left too long after mixing, causing copolymer particles to form between the paint and hardener; too little paint output from the spray gun and excessive pressure, resulting in poor paint atomization or the spray gun being too close to the surface.

    Solution: Clean the paint spray room, cover the paint buckets; mix the paint properly, avoid leaving it for too long; adjust the spray gun to ensure optimal working condition, and set the nozzle distance from the surface to be between 20-50 cm.

    2. Phenomenon: Drizzle

    Reason: A Teflon Coating Expert Explains - Too much thinner causes the paint to have low viscosity and lose adhesion; excessive oil output, too close to the surface or the spray speed is too slow; too much paint applied each time or too short intervals between re-spraying; uneven surface, especially streamlined shapes prone to sagging.

    Solution: Mix according to specifications; control the oil output to ensure increased spray gun speed; do not apply too thick a coat of paint, two coats with an interval between them are ideal; control the oil output to reduce film thickness; mix as per instructions.

    3. Phenomenon: Orange Peel

    Reason: A Teflon Coating Expert Explains That Too Much hardener causes the paint film to dry too quickly and react violently; excessive spray pressure wrinkles the paint film, preventing it from leveling; and high temperatures in the work area lead to剧烈 reaction of the paint film.

    Solution: Follow the instructions for mixing ratio; adjust the pressure, not too high; and pay attention to the site temperature, consider adding a slow-drying thinner to control the drying speed.



Contact us

Chongqing Zhijiu Technology Co., Ltd.
Service Hotline 18584567111
Company Phone 18996339088
Company Address 8 Tieshan Road, Biquan Street, Bishan District, Chongqing

Message Consultation

 Click OK to indicate that you agree to《Service terms》《Privacy policy》

www.114global.com © Zhongshang 114 Hebei Network Technology Co., Ltd.Address: Room 6009, Oriental New World Center, No.118 East Zhongshan Road, Qiaoxi District, Shijiazhuang City, Hebei ProvincePlatform Service Hotline: 4006299930

 Click OK to indicate that you agree to《Service terms》《Privacy policy》